Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Orgalloy® RS 6630 BLACK - PA66-GF30... - ARKEMA

Material Data Center offers the following functions for Orgalloy® RS 6630 BLACK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Orgalloy R datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Orgalloy® RS 6630 BLACK resin is a fiberglass reinforced polyamide 66 alloy designed for injection molding. This black grade offers an outstanding dimensional stability, chemical resistance to automotive fluids and is ideal for the realization of complex parts.

Main applications:
  • Electric connectors
  • Sport parts
  • Automotive fan shrouds

Packaging:
This grade is delivered dried in sealed packaging (25kg bags) ready to be processed.

Shelf life:
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 8.5 / * cm³/10min ISO 1133
Temperature 275 / * °C -
Load 2.16 / * kg -
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 8600 / 8300 MPa ISO 527
Stress at break 129 / 125 MPa ISO 527
Strain at break 2.6 / 3 % ISO 527
Tensile creep modulus, 1h * / 7900 MPa ISO 899-1
Tensile creep modulus, 1000h * / 5620 MPa ISO 899-1
Charpy impact strength, +23°C 58 / 58 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 50 / 50 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 10 / 11 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 9 / 9 kJ/m² ISO 179/1eA
Shore D hardness 79 / * - ISO 7619-1
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 255 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 237 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 257 / * °C ISO 75-1/-2
Vicat softening temperature, B 204 / * °C ISO 306
Coeff. of linear therm. expansion, parallel 18 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 110 / * E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB / * class IEC 60695-11-10
Thickness tested 1.6 / * mm -
Burning Behav. at thickness h HB / * class IEC 60695-11-10
Thickness tested 3.2 / * mm -
Electrical propertiesdry / condUnitTest Standard
ISO Data
Relative permittivity, 100Hz - / 3 - IEC 62631-2-1
Relative permittivity, 1MHz - / 4 - IEC 62631-2-1
Dissipation factor, 100Hz - / 290 E-4 IEC 62631-2-1
Dissipation factor, 1MHz - / 160 E-4 IEC 62631-2-1
Volume resistivity - / >1E13 Ohm*m IEC 62631-3-1
Surface resistivity * / >1E15 Ohm IEC 62631-3-2
Electric strength 34 / 34 kV/mm IEC 60243-1
Comparative tracking index * / 600 - IEC 60112
Other propertiesdry / condUnitTest Standard
Water absorption 3.9 / * % Sim. to ISO 62
Humidity absorption 1.3 / * % Sim. to ISO 62
Density 1270 / 1270 kg/m³ ISO 1183
Processing Recommendation Injection MoldingValueUnitTest Standard
Pre-drying - Temperature 80 °C -
Pre-drying - Time 4 - 8 h -
Melt temperature 270 - 290 °C -
Mold temperature 60 - 80 °C -
Diagrams
Viscosity-shear rate , Orgalloy® RS 6630 BLACK, PA66-GF30..., ARKEMA
Shearstress-shear rate , Orgalloy® RS 6630 BLACK, PA66-GF30..., ARKEMA
Dynamic Shear modulus-temperature , Orgalloy® RS 6630 BLACK (dry), PA66-GF30..., ARKEMA
Characteristics
Processing
Injection Molding
Delivery form
Pellets, Black
Special Characteristics
Light stabilized or stable to light, Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding
Processing conditions:
- Drying time (only necessary for bags opened for more than two hours): 4-8 hours at 80°C
- Injection temperature (min-recommended-max): 270-280-290°C 
- Mould temperature (min-max): 60-80°C 
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com